Smoothing method for cleaved films made using a release layer
Granted 21 May 2002 · 1 office action
Assignee: Silicon Genesis
Law firm: Law firm · Log in to unlock
Attorney: Attorney · Log in to unlock
Inventors: Sien G. Kang, Igor J. Malik · Examiner: Randy Gulakowski
Life of the application
8 dated eventsAbstract
A method for treating a film of material, which can be defined on a substrate, e.g., silicon. The method includes providing a substrate comprising a cleaved surface, which had a porous silicon layer thereon. The substrate may have a distribution of hydrogen bearing particles defined from the cleaved surface to a region underlying said cleaved surface. The method also includes increasing a temperature of the cleaved surface to greater than about 1,000 Degrees Celsius while maintaining the cleaved surface in a etchant bearing environment to reduce a surface roughness value by about fifty percent and greater. Preferably, the value can be reduced by about eighty or ninety percent and greater, depending upon the embodiment.
Claims as granted
29 claimsLog in to read the claims of this application.
Log in to unlockClassifications
10 codes- H01L2/176
Claim changes
SoonSee which claims were amended, added or cancelled during examination, with every added and removed word marked.
The published claims of this application are not paired with the granted ones in what we hold.
File wrapper
See the full prosecution history — every USPTO and applicant action on this file, in order.
Log in to unlockDocuments
Log in to open the documents of this file: the application as filed, every office action and response, the notice of allowance.
Log in to unlockChain of title
See the full assignment history — every owner this patent has passed through, with recordation dates and reel/frame numbers.
Log in to unlock